Superalloy | GH90, GH1131, GH1140, GH131, GH188, GH2026, GH2132, GH2136, GH2747, GH2901, GH2901, GH30, GH3007, GH3030, GH3044, GH3128, GH3304, GH3308, GH3536, GH3600, GH3625, GH4049, GH4080A, GH4090, GH4099, GH4141, GH4145, GH4169, GH4738, GH5188, GH5605, GH5K, GH600, GH605, GH625, GH738, GH747, GH80A, GH901 |
Thickness | 0.3-200mm |
Width | 40mm-600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc |
Length | 2000mm, 2500mm, 3000mm, 5800mm, 6000mm, 12000mm, etc |
Standard | ASTM, JIS, AISI, GB, DIN, EN |
Certification | ISO, SGS, BV and so on. |
Technique | Cold Rolled, Hot Rolled |
Edge | Mill Edge Slit Edge UNS No Generic term Composition |
DIN/EN | UNS No | Generic term | Composition |
---|---|---|---|
2.4819 | N10276 | Hastelloy C-276 | 57Ni-16Mo-16Cr-5Fe-4W-2.5Co-1Mn-0.35V-0.08Si-0.01C |
2.461 | N06455 | Hastelloy C-4 | 65Ni-16Cr-16Mo-0.7Ti-3Fe-2Co-1Mn-0.08Si-0.01C |
2.4602 | N06022 | Hastelloy C-22 | 56Ni-22Cr-13Mo-3Fe-2.5Co-0.5Mn-0.35V-0.08Si-0.01C |
2.4675 | N06200 | Hastelloy C-2000 | 59Ni-23Cr-16Mo-1.6Cu-0.08Si-0.01C |
2.4665 | N06002 | Hastelloy X | 47Ni-22Cr-18Fe-9Mo-1.5Co-0.6W-0.1C-1mn-1Si-0.008B |
2.4617 | N10665 | Hastelloy B-2 | 69Ni-28Mo-0.5Cr-1.8Fe-3W-1.0Co-1.0Mn-0.01C |
2.466 | N10675 | Hastelloy B-3 | 65Ni-28.5Mo-1.5Cr-1.5Fe-3W-3Co-3Mn-0.01C |
N06030 | Hastelloy G-30 | 43Ni-30Cr-15Fe-5.5Mo-2.5W-5Co-2Cu-1.5Mn-0.03C | |
N06035 | Hastelloy G-35 | 58Ni-33Cr-8Mo-2Fe-0.6Si-0.3Cu-0.03C |
We are manufacturer. Every month, we do a procurement for a massive number of steel material from Chinese state owned mill. The total value of steel processing equipment is more than 30 million dollars. Our major products cover carbon steel, stainless steel, galvanized steel, and PPGI / PPGL, and it is totally compatible to all kind of world steel standard.
Yes, we do. In large-scale indoor warehouses, the total stock value is over 150 millions dollar.
It is free, depend on the value of the sample. The cost of the freight would be charge.
Officially, it is within 7 days. Actually, we can deliver within 3 days. Customized products or non-standard size products would be taken 10-30 days to deliver, depend on the production cycle. Generally, most of the products finished and delivered within 20 days.
We are so confident that we can deliver goods on time. In experience of steel supply chain for over 15 years, we have built a perfect supply chain system which can provide a variety of supply solutions and rapidly respond services for international buyers.
© 2024 SHANDONG TISCO STEEL CO.,LTD. All Rights Reserved.